Title:
Grafting of 4-aminoantipyrine from guar gum substrates using graft atom transfer radical polymerization (ATRP) process

dc.contributor.authorVivek Mishra
dc.contributor.authorRajesh Kumar
dc.date.accessioned2026-02-07T05:26:45Z
dc.date.issued2011
dc.description.abstractATRP graft copolymerization of 4-aminoantipyrine (AAP) was carried out successfully at 50 °C from a guar gum based macroinitiator (GGBr), Cu(I)Br and 2,2′-bipyridyl(bpy) as initiator, catalyst and ligand, respectively, in water. Factors affecting the conversion and rate of graft copolymerization such as temperature, concentration of monomer, catalyst, ligand and initiator were studied. The best initial molar concentration ratio of [AAP]:[GGBr]:[Cu(I) Br]:[bpy] was found 100:1:1:2 for controlled graft copolymerization. The plot ln[M]0/[M]t vs. time showed first order kinetics with respect to 4-aminoantipyrine. The activation energy (Ea = 25.15 kJ mol-1), enthalpy of activation (ΔH‡ = 22.42 kJ mol-1) and negative value of entropy of transition state (ΔS‡ = -233.82 J mol-1 K-1) support the progress of polymerization reaction. The % grafting ratio was found to be 5184% and the graft copolymer was characterised by 1H NMR, FTIR, UV, GPC, XRD, TGA and DSC analyses. © 2011 Elsevier Ltd All rights reserved.
dc.identifier.doi10.1016/j.carbpol.2011.04.052
dc.identifier.issn1448617
dc.identifier.urihttps://doi.org/10.1016/j.carbpol.2011.04.052
dc.identifier.urihttps://dl.bhu.ac.in/bhuir/handle/123456789/22676
dc.subject4-Aminoantipyrine
dc.subjectATRP graft copolymer
dc.subjectGuar gum
dc.subjectThermal analysis
dc.titleGrafting of 4-aminoantipyrine from guar gum substrates using graft atom transfer radical polymerization (ATRP) process
dc.typePublication
dspace.entity.typeArticle